I have a quick technical question. My goal is to increase the gloss of the Rutile at 60 degrees.
My attempted solution is
1. To modify the process, I assume I could lower the temperature during the coating process or the drying process ( for sulphate process).
2. Or I could increase the Al2O3 coating percentage to enhance dispersion to create space particle.
Anyone who has more experienced got a better idea on this? Thanks.