How about this procedure? :
http://rockyledgemining.tripod.com/solventexchange.htmlProcedure:
1. Prepare 1 parts of clear leach by filtering pregnant solution through a # 42 Whatman filter into the beaker marked Gold. [NOTE: You may rinse the debris from the filtering back into your original leaching container to retain any unleached metals.]
2. Add 1 parts of distilled water and stir manually (stirring rod or agitating the beaker)
3. Add 2 parts of CDE 5 Gold Collector.
4. Place beaker on a magnetic stirring hotplate, place stir bar in the beaker and agitate strongly for 45 minutes at 98 degrees F.
5. Transfer the solution to a separatory funnel and allow it to settle into two layers. The gold will be in the top layer.
6. Drain the bottom layer into a beaker marked “Pregnant solution minus Au” and set it aside. [This “waste” liquid will be processed later for possible platinum group metals. The procedure is the same, but the collectors and strippers and different for each metal. Supplies may be purchased from Rocky Ledge.]
7. Place the CDE 5 into a beaker and add an equal amount of CDE 9 gold separator.
8. Agitate vigorously while bringing the solution to 180 F. This could take as long as 90 minutes depending on the volume as well as your heating and stirring equipment.
9. As the temperature rises a color change in the liquid will become apparent.
10. At approximately 180 F any gold present will appear to be “black” particulate floating in the solution. When the color is no longer modifying stop the heating and stirring.
11. Place the solution into a separatory funnel and allow to separate.
12. Drain the bottom solution through a # 42 Whatman filter to collect the gold particulate.
13. Rinse the particulate from the filter paper into an appropriate beaker. Add a small amount of HCL to the liquid and stir vigorously.
14. An amount of the gold will be “in the vortex” created by the stirring. Slowly add isopropyl alcohol—store-bought cheap rubbing alcohol—to the dilute HCL solution. When the mix is approximately 50/50 the gold will fall out of the vortex and settle in the bottom.
15. Air dry the powder in a protected area. You can be assured the material remaining is an ultra high quality gold in sponge form. This sponge gold is sale-able as it is.
Can anybody explain above procedure?