Thanks a lot my friends for your replays.
Even I don't use ethylen glycol, which means that starter materials are La Co Ni nitrates and citric acid, the material go away from its recipient when I put it inner the muffle, at 1C/min, until 500C. So I have become to believe that it phenomenon is due to hydration during its storage, which is about 5 days. Why do you think?, Is it correct?. Can you tell me some reference to learn more about it problem?
Best Regards.
Pablo