Hello,
I was preparing Copper acetate from 40ml 9% destilled winegar, 50ml 3% hydrogen peroxide (pharm grade) and 2,75g copper wire. After 24h about 0,5g of copper dissolved into solution, which was clear and deep blue color. I start evaporating it in hot water bath, but now after 2 hours white precipate formed on the bottom of the flask.
My question is, where does the white color from?
I used the copper wire as anode in previous electrolytic experiment preparing the same product as now. I washed it, but not completely. I did filter the solution using a paper towel, which I rinsed very well. Maybe one of above causes introduced impurities. Which is more possible and why?