Hi
We have a problem on our glue (at chipboard production) i wrote the results and the glue specifications below:
A sample formula experiment and results at 180 degrees:
55% glue 40 liter
25% ammonia 0.325 liters
1% water 3.5 liter
gel -55
Result: the gel time was observed short, the speed of the press was long, and manufacturing errors occurred
UREA FORMALDEHYDE RESIN L18 / 15-N
PRODUCT SPECIFICATION
Appearance Milk white Solids, 65 ± 1.0% Lab 5.11.03.01 Density, g / cm3, 20 ° C 1,270 - 1,290 Viscosity, cPs, 20 ° C 400 - 800 Lab pH, 20 ° C 7.5 - 9.0 Reactivity, s, 100 ° C 35 - 45 Free Formaldehyde, 0.30% max.
Anyone can help us to identify the bit a of a problem?